Ladle, tundish nozzles and
well blocks
|
Item |
Chrome Corundum Nozzle |
Corundum Nozzle |
Al2O3-SiC-C Nozzle |
Spinel-C Nozzle |
LT-70
Nozzle |
LT-85
Nozzle |
Upper
Porous nozzle for tundish |
|
Al2O3
(%)− |
90 |
93 |
65 |
55 |
70 |
85 |
80 |
|
Cr2O3
(%)− |
2.5 |
|
|
13(MgO) |
|
|
2.5 |
|
C (%)− |
|
|
7 |
10 |
7 |
3 |
|
|
A.P.
(%)+ |
22 |
24 |
8(Impre-gnated) |
8(Impre-gnated) |
15 |
15 |
24 |
|
B.D.
(g/cm3)
− |
2.9 |
2.95 |
2.7 |
2.7 |
2.7 |
2.9 |
|
|
Refractoriness (≧)
− |
1790 |
1790 |
|
|
|
|
|
|
Linear change on reheating(%) |
1550≧x3h
+0.1-+0.3 |
1600≧x3h
+/-0.5 |
|
|
|
|
|
|
|